我再K文件*mat-erosion
*MAT_ADD_EROSION(两个卡片,总共12个参数)
CARD1
MID EXCL MXPRES MNPEPS
CARD2
PFAIL SIGPL(最大主应力) SIGVM EPSPL (最大主应变) EPSSH SIGTH IMPULSE FAILTM
部分中作出了如下设置了:
*MAT_PLASTIC_KINEMATIC
1,0.250E+04,0.300E+11,0.200000,2.0E+7,0.0,0.0
*MAT_BRITTLE_DAMAGE(96号整体式砼材料)
2,2500,0.300E+11,0.200000,6.00E+06,1.40E+7,0.5E+06,0.03
0.724E+06,0.050,0.200E+12,3.35E+08,1.1E+10,0.1,30.0E+06
*MAT_BRITTLE_DAMAGE
3,2500,0.300E+11,0.200000,6.00E+06,1.40E+7,0.5E+06,0.03
0.724E+06,0.050,0.200E+12,3.35E+08,1.1E+10,0.025,30.0E+06
$
*mat_add_erosion
2,567
567,3.0E+7(最大主应力),567,0.015(最大主应变),567,567,567,567
$
*mat_add_erosion
3,567
567,567,567,567,567,567,567,0.5(失效时间)
我之前也分别设置了最大主应力和最大主应变的值,材料失效是的值也对应不上,请问怎么回事?