takikoyx 发表于 2009-3-6 13:20:35

请高手帮我看看我这个分析问题出在哪

我做了一块玻璃板的受热膨胀分析,我将板的四周设uz方向约束,参考温度303K,处于403k的温度下,稳态分析,用solid5单元,为什么做出来的结果膨胀得不对称,而且每次结果膨胀的方向都不一样,还是说不需要用热-结构耦合,直接用结构分析就行了?而且为什么用solid5单元它用非线性的计算了
/PREP7
!*
ET,1,SOLID5
!*
TOFFST,0
!*
MPDATA,DENS,1,,2.51e-6
MPDATA,EX,1,,72900
MPDATA,PRXY,1,,0.208
MPDATA,ALPX,1,,7.2e-6   
MPDATA,KXX,1,,0.00096   
SAVE
TYPE,   1   
MAT,       1
REAL,   
ESYS,       0   
SECNUM,
!*
ESIZE,0.03,0,   
CM,_Y,VOLU
VSEL, , , ,       1
CM,_Y1,VOLU
CHKMSH,'VOLU'   
CMSEL,S,_Y
!*
VSWEEP,_Y1
!*
CMDELE,_Y   
CMDELE,_Y1
CMDELE,_Y2
!*
SAVE
FINISH
/SOL
!*
ANTYPE,0
TREF,303,   
FLST,2,4,5,ORDE,3   
FITEM,2,2   
FITEM,2,4   
FITEM,2,-6
!*
/GO
DA,P51X,UZ,
TUNIF,403,
SAVE
/STATUS,SOLU
SOLVE

takikoyx 发表于 2009-3-6 13:25:47

http://home.simwe.com/attachment/200903/6/362117_1236317113ncm9.jpg 1# takikoyx
结果图,合位移
页: [1]