巷道锚杆支护的问题
用实验室力学测试得到的参数来模拟,不打锚杆巷道变形量也很小,是什么问题呢2d的
有没有经验的参数呢?比如把岩性怎么调能够得到理想的效果 参数拿出来看看 先谢谢了,请帮忙看看。
new
grid 150,150
model elastic
set large
;加密重点部分网格
;第一步
gen 0,0 0,20 20,20 20,0 i=1,26 j=1,26
gen 20,0 20,20 40,20 40,0 i=26,126 j=1,26
gen 40,0 40,20 60,20 60,0 i=126,151 j=1,26
;第二步
gen 0,20 0,40 20,40 20,20 i=1,26 j=26,126
gen 20,20 20,40 40,40 40,20 i=26,126 j=26,126
gen 40,20 40,40 60,40 60,20 i=126,151 j=26,126
;第三步
gen 0,40 0,60 20,60 20,40 i=1,26 j=126,151
gen 20,40 20,60 40,60 40,40 i=26,126 j=126,151
gen 40,40 40,60 60,60 60,40 i=126,151 j=126,151
;形成巷道(4.4*3.0 m)
gen line 27.8,28.2 27.8,31.2
gen line 27.8,31.2 32.2 31.2
gen line 32.2 31.2 32.2 28.2
gen line 32.2 28.2 27.8,28.2
gen adjuist
;边界条件
fix x i=1
fix x i=151
fix y j=1
ini syy=-10e6
ini sxx=-5e6
ini szz=-5e6
app syy=-10e6 j=151
his nstep=100
his ydis i=76 j=82
prop D=2500 S=13.68e9 B=24.54e9
set g=10
his unbal
solve
plot his 1
save bdmodel-1.sav
rest bdmodel-1.sav
model mohr
win 20 40 20 40
;老顶
prop D=2583 S=34.63e9 B=48.16e9 C=28e6 F=36.17 T=9.70e6 j=1 67
;直接顶
prop D=2581 S=31.43e9 B=64.36e9 C=39.5e6 F=26.49 T=9.22e6 j=67 84
;煤
prop D=1420 S=5.28e9 B=12.9e9 C=8.2e6 F=30.24 T=3.37e6 j=84 95
;底板
prop D=2643 S=39.29e9 B=57.7e9 C=26e6 F=23.89 T=8.18e6 j=95 151
;挖巷道
ini xdis=0 ydis=0
ini xvel=0 yvel=0
model null reg 76,76
solve
save bdmodel-2.sav 我刚开始学习FLAC。各位大侠,请指教izhy2008@cumt.edu.cn
如有例子麻烦给发一份,不胜感激 这么强的岩石放到这么小的初始应力下,变形肯定很小。
对于煤矿来讲,岩体参数偏大太多。 tg0215 版主常回来看看! 我也感觉岩石的强度和岩体的强度有区别,但是到底怎么换算呢?数值模拟中参数到底怎么设置呢? 岩体强度和岩石强度是由很大差别的
实验室得到是岩石的强度
不可以直接用在数值实验的 那到底怎么办呢? 把参数调小就可以了 你的参数太大每次减小1/3 10楼的方法效果很明显,不知道有没有什么依据?就是感觉心里没底 有待学习学习啊 刚开始学就要用 估计是地应力太小了 觉得岩体的强度很大
应该适当的弱化下
可以参考矿大那本关于数值模拟的书 !!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!!